| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | |
|
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite
Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet..
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
|
Network Polymers PC-1015R
Description: Natural PolycarbonateInformation provided by Network Polymers Inc.
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Thickness 3.17 mm
|
16.0
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)&
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Temperature 22.8 °C
|
16.0
ft-lb/in <br>@Temperature 73.0 °F
|
ASTM D256 |
|
Polymer Resources NY66-IM2 Impact Modified Nylon 66
Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are ..
|
|||
| Izod Impact, Notched | 8.52 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific)
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color..
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Temperature -30.0 °C
|
16.0
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin
(discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Temperature -30.0 °C
|
16.0
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
DuPont Bexloy® AXW504BK Modified Ionomer Resin
(discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B..
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF..
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
M. Holland Company PC518R Polycarbonate
High clarityUltra high impact resistanceGood mold releaseApplications: AppliancesFood containersTable products
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Global PC-1603 Standard Grade Polycarbonate
Information provided by Global Polymers Corporation.
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Temperature 22.8 °C
|
16.0
ft-lb/in <br>@Temperature 73.0 °F
|
0.125"; ASTM D256 |
|
LTL Color Compounds ColorRxâ„¢ PC-1001A Antimicrobial Polycarbonate
A 10 melt grade of Polycarbonate containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders..
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Thickness 3.17 mm
|
16.0
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES Elastoblend® PA6 IM HS L BK
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUL File Number: E157318Processing Method: In..
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Thickness 3.17 mm
|
16.0
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES Elastoblend® PA6 IM L W N
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Thickness 3.17 mm
|
16.0
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES Elastoblend® PA6 IM X
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat..
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Thickness 3.17 mm,<br> Temperature 22.8 °C
|
16.0
ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.0 °F
|
Compression Molded; ASTM D256 |
|
Teknor Apex APEX® RE 9016A Polyvinyl Chloride, Rigid
Features: Good Weather Resistance; High Impact Resistance Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM Data |
|
Styron CALIBREâ„¢ 701 15 Polycarbonate, General Purpose
CALIBRE® 701 series polycarbonate resins are a general purpose, transparent, ignition resistant grades equipped with a mold release package. The CALIBRE 701 series resins exhibit a high heat resi..
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Teknor Apex Synres® PP G20 62 Polypropylene, Glass Reinforced
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many ..
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | At 73°F; ASTM D256 |
|
Plastics Group Polifil® 627L Nylon 6/6 (DAM)
Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group...
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Chase Plastics CP Pryme® N100STL (DAM) Nylon 6, Super Toughened, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Thickness 3.17 mm
|
16.0
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Diamond Polymers NPP25-0116 Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Applied Composites 8092 Polyester SMC
Industry Application: ConstructionProduct Application: Building ProductsDistinct Features: Pigmentable, High Molding Efficiency, Low Thermal ExpansionInformation provided by Applied Composites Corpo..
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Aaron Industries AAROPRENE® AEPC 5000-2 Engineered Polycarbonate Resin
Melt flow index may be specified.
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Ashley Polymers Ashlene® 1041R Polycarbonate
A general purpose, injection molding grade, natural resin.Data provided by the manufacturer
|
|||
| Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
|
Ashley Polymers Ashlene® TD930H Nylon 12
A plasticized Nylon 12 offering outstanding flexibility with superior moisture and chemical resistance, UV and heat stabilized for weatherability.Data provided by the manufacturer
|
|||
| Izod Impact, Notched |
8.54
J/cm <br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
|
16.0
ft-lb/in <br>@Thickness 0.250 in,<br> Temperature 73.4 °F
|
Method A, Injection Molded; ASTM D256 |
|
PolyOne Edgetek® UR-20CF/000 Thermoplastic Elastomer - TPU, Carbon Fiber Reinforced
(discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||