Chengdu Polyster H3303 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H3303 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance at low temperatures. Moldable even in thin sections. Can be used in light-colored products. Applications requiring flex life coupled with good flexibility at low temperatures, such as hose, wires, cables and optical fiber. For blending with PVC to improve the mechanical properties.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Melt Flow 8.0 - 12 g/10 min
8.0 - 12 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
ISO 868
Tensile Strength, Ultimate 18.0 MPa
2610 psi
ISO 527-1
Elongation at Break 550 %
550 %
ISO 527-1
Flexural Modulus 0.0400 GPa
5.80 ksi
ISO 178
Tear Strength 70.0 kN/m
399 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974