| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.35 g/cc | 1.35 g/cc | silicone property; Arlon SQA-TMS-024 |
| Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
| 152 microns | 6.00 mil | side 2; Arlon SQA-TMS-003 | |
| 406 microns | 16.0 mil | substrate; Arlon SQA-TMS-003 | |
| 711 microns | 28.0 mil | overall; Arlon SQA-TMS-003 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 60 | 60 | silicone property; ASTM D2240 |
| Tensile Strength, Ultimate | 5.52 MPa | 800 psi | silicone property; ASTM D412 |
| Elongation at Break | 225 % | 225 % | silicone property; ASTM D412 |
| Adhesive Bond Strength | 0.0552 MPa | 8.00 psi | Arlon SQA-TMS-011 |
| Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
| UL RTI, Electrical | 200 °C | 392 °F | |
| UL RTI, Mechanical without Impact | 200 °C | 392 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 120 min <br>@Temperature 204 °C |
2.00 hour <br>@Temperature 400 °F |
|
| 15.0 min <br>@Pressure 0.345 MPa,<br> Temperature 121 °C |
0.250 hour <br>@Pressure 50.0 psi,<br> Temperature 250 °F |
||
| Shelf Life | 6.00 Month <br>@Temperature 23.9 °C |
6.00 Month <br>@Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Red |