| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | Silicone Property; Arlon SQA-TMS-024 |
| Thickness | 50.8 microns | 2.00 mil | silicone; Arlon SQA-TMS-003 |
| 102 microns | 4.00 mil | substrate; Arlon SQA-TMS-003 | |
| 152 microns | 6.00 mil | overall; Arlon SQA-TMS-003 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 60 | 60 | Silicone Property; ASTM D2240 |
| Tensile Strength, Ultimate | 5.72 MPa | 830 psi | Silicone Property; ASTM D412 |
| Elongation at Break | 150 % | 150 % | Silicone Property; ASTM D412 |
| Tear Strength | 9.64 kN/m | 55.0 pli | Silicone, Die B; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 59.65 kV/mm | 1515 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 120 min @Temperature 204 °C |
2.00 hour @Temperature 400 °F |
|
| Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Char length (inches) | 0.25 | FAR 25.853 App.F, P.1, S.Aii |
| Color | Red | |
| Flame and Glow Resistance (seconds) | 1 | FAR 25.853 App.F, P.1, S.Aii |