Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Extrusion/Tubing Grade
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical resistance. Easy to be processed.Example applications: Pneumatic control tubes, Fuel line.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 1.2 %
1.2 %
Melt Flow 5.6 g/10 min

@Load 2.16 kg,
Temperature 235 °C
5.6 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 24 %
24 %
50 mm/min
Tensile Modulus 0.465 GPa
67.4 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 168 °C
334 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in