Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SCG Chemicals EL-Leneâ„¢ M9001 Butene (C4) Rotational Molding Resin

Category Polymer , Thermoplastic
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ M9001 Butene (C4) Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Natural base resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such as medium-to-large water tanks, (5,000-22,500 liters), underground tanks, septic tanks, manholesInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.938 g/cc
0.938 g/cc
ASTM D1505
Melt Flow 3.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 1100 %
1100 %
ASTM D368
Flexural Modulus 0.750 GPa
109 ksi
ASTM D790
Dart Drop Total Energy 2.50 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00468 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
Thermal Properties Metric English Comments
Melting Point 127 °C
261 °F
ASTM D2117
Crystallization Temperature 113 °C
235 °F
ASTM D2117
Descriptive Properties Value Comments
Food Contact Approved FDA, AS/NZS 4020, and AS/NZS 4766
Heavy Metal Free (Base Resin) Yes
Peak Internal Air Temperature 200°C
TPE Method
Shrinkage Level medium
TPE Method
UV Stabilizer UV-8 & Low UV
ASTM G155
Users viewing this material also viewed the following: