Arkema Group Lucalor® RY 123 CPVC, Plumbing Grade

Category Polymer , Thermoplastic , Vinyl (PVC) , Chlorinated PVC (CPVC)
Manufacturer Arkema
Trade Name Lucalor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Lucalor® RY 123 CPVC, Plumbing Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LUCALOR RY 123 is a chlorinated polyvinyl chloride compound (CPVC) developed for the injection molding of fittings for hot water supply.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.0 MPa
7690 psi
50 mm/min
Elongation at Break 32 %
32 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %
5.0 %
50 mm/min
Tensile Modulus 2.62 GPa
380 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
Vicat Softening Point 106 °C
223 °F
50°C/hr; 50N
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Oxygen Index 65 %
65 %