Type: Estane® ALR E87A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
ASTM D2240
Tensile Strength, Ultimate 53.1 MPa
7700 psi
ASTM D412
Elongation at Break 390 %
390 %
ASTM D412
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D412
200% Modulus 0.0131 GPa
1.90 ksi
ASTM D412
300% Modulus 0.0296 GPa
4.30 ksi
ASTM D412
Flexural Modulus 0.0221 GPa
3.20 ksi
ASTM D790