Chosun Refractories COD-2 Special brick

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories COD-2 Special brick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.10 g/cc
0.0759 lb/in³
Porosity 15 %
15 %
Mechanical Properties Metric English Comments
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 3.00 µm/m-°C

@Temperature 1000 °C
1.67 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 36 %
36 %
MgO 5.0 %
5.0 %
Descriptive Properties Value Comments
Refractories Under Load(2kg/?,T2?) 1,350