Arkema Group KYNAR® LBG2 Polyvinylidene Fluoride Powder

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Arkema
Trade Name KYNAR®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group KYNAR® LBG2 Polyvinylidene Fluoride Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc.
Physical Properties Metric English Comments
Bulk Density 0.288 g/cc
0.0104 lb/in³
Particle Size 5.0 µm
5.0 µm
Loosely agglomerated
Particle Mesh Size 14 Mesh
14 Mesh
Viscosity 3.30e+6 - 3.90e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
3.30e+6 - 3.90e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Melt Flow 3.0 - 8.0 g/10 min

@Load 21.6 kg,
Temperature 232 °C
3.0 - 8.0 g/10 min

@Load 47.6 lb,
Temperature 450 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 151 - 155 °C
304 - 311 °F