CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coating available5 strategic manufacturing locationsPropertiesRecycled contentAgricultural and other non-FDA applicationsCost effective solutionExcellent yieldInformation provided by Alcoa Kama Co.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Thickness 178 - 1520 microns
7.00 - 60.0 mil
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 10.3 MPa
>= 1500 psi
ASTM D638
Elongation at Break >= 20 %
>= 20 %
ASTM D638
Flexural Modulus >= 1.31 GPa
>= 190 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Processing Properties Metric English Comments
Processing Temperature 127 - 166 °C
260 - 330 °F
Thermoforming Temp
Descriptive Properties Value Comments
Resistance to Acid Good to Excellent
Resistance to Alcohols Good to Excellent
Resistance to Alkalis Excellent
Resistance to Fat, Grease, and Oil Good
Resistance to Hydrocarbon Solvents Poor
Resistance to Strong Oxidizers Poor
Yield, in²/lb/mil 26360