Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L 9561 PPS, 60% Glass Fiber/Mineral  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.94 g/cc
0.0701 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
DIN 53 455
Elongation at Break 1.2 %
1.2 %
DIN 53 455
Modulus of Elasticity 14.0 GPa
2030 ksi
DIN 53 457
Flexural Yield Strength 130 MPa
18900 psi
DIN 53 452
Flexural Modulus 14.0 GPa
2030 ksi
DIN 53 457
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Comparative Tracking Index 150 V
150 V
IEC 112
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F