ExxonMobil LL Mobiltac Double Letter Series

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL Mobiltac Double Letter Series.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Mobiltac Double Letter Series products are high performance, non-diluent type, heavy-bodied products intended for the lubrication of open gears over a wide range of environmental conditions and machine requirements. They incorporate extreme pressure additives for the protection of gear teeth and metal surfaces subject to extremely heavy loads. They form a cohesive and adhesive lubricating film that resists wear, water wash and excessive "throw off". They lubricate properly under boundary conditions. They resist peeling or flaking at sub-zero temperatures. Mobiltac Double Letter Series lubricants are recommended for all-purpose applications in open gears. The two lighter grades meet many builder requirements for heavily loaded splash-type enclosed gearing.Mobiltac Double Letter Series lubricants are recommended for all-purpose applications in open gears. The two lighter grades are used in heavily loaded splash-type enclosed gearing. Applications include: Machinery components as hoist gears, swing gears, large press gears; Equipment in forge shops, pit or strip mining; Large earthmoving equipment and cement kilns
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 1209 cSt
1209 cSt
ASTM D445
Thermal Properties Metric English Comments
Flash Point 182 °C
360 °F
ASTM D92