Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 14.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
PolyOne OnForce™ LFT NN-50LGF/000 HS Natural Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Flexural Modulus 14.0 GPa
2030 ksi
Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound for the encapsulation of semiconductor devices and fiber optics. Excellent moldability (good release, ..
Flexural Modulus 14.0 GPa
2030 ksi
Cookson Group Plaskon® SMT-B-1™ Epoxy Molding Compound for PBGAs  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA). It is formulated with a unique resin system that min..
Flexural Modulus 14.0 GPa
2030 ksi
Cookson Group Plaskon® ULS-12 Epoxy Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i..
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
DSM Akulon® K-FHG0 (Dry) 50% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Flexural Modulus 14.0 GPa
2030 ksi
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo..
Flexural Modulus 14.0 GPa
2030 ksi
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Flexural Modulus 14.0 GPa
2030 ksi
Lehmann & Voss LUVOCOM® 80-7050 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Flexural Modulus 14.0 GPa
2030 ksi
1.3 mm/min; ASTM D790
Lavergne VYPET VNT 645 PET 45% Glass Reinforced
Vypet VNT 645 is a 45% glass reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Excellent strength and stiffness; E..
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Solvay Specialty Polymers Ryton® R-4-240BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Solvay Specialty Polymers Ryton® R-4-280NA Polyphenylene Sulfide (PPS), Glass Fiber
Ryton® R-4-280NA 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis..
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn..
Flexural Modulus 14.0 GPa
2030 ksi
Cosmic Plastics E4940 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade
Data provided by the manufacturer.
Flexural Modulus 14.0 GPa
2030 ksi
ASTM-D790
Polyram PB302G50 Nylon 6, 50% Glass Fiber
50% glass fiber reinforced, UV and heat stabilized polyamide approved and listed by W.R.C potable water and NSF/ANSI61 internationalInformation provided by Polyram Ram On Ind.
Flexural Modulus 14.0 - 19.0 GPa
2030 - 2760 ksi
ISO 178
Vyncolit 3640 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Polyram PlusTek PB302G50BK39P Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized
50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram.
Flexural Modulus 14.0 GPa
2030 ksi
Cosmic Plastics E4920 Mineral Filled Epoxy Molding Compound, Encapsulated Grade
Data provided by the manufacturer.
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Polyram PlusTek PB302G50BK39D Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized
50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram.
Flexural Modulus 14.0 GPa
2030 ksi
ASTM D790
E-Polymers SEPAZ® C230GP 30% Glass Fiber Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Flexural Modulus 14.0 GPa
2030 ksi
dry; ISO 178
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced
50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
CENTROPLAST CENTROTRON GF 40 Polyphenylene sulfide 40% glass fiber
CENTROTRON GF is a plastic that is reinforced for high strength and rigidity, that can be used at high operating temperatures. Applications include bearings, sealing rings, rods and hollow bars. In..
Flexural Modulus 14.0 GPa

@Temperature 23.0 °C
2030 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Rynite® 545 BK504 PET  (Unverified Data**)
Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont..
Flexural Modulus 14.0 GPa
2030 ksi
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
Flexural Modulus 14.0 GPa

@Temperature 23.0 °C
2030 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers.
Copyright © lookpolymers.com All Rights Reserved