Price EMAIL US    sales@lookpolymers.com
Material Notes:
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ContainersProcessing: Injection Molding (Melt Temperature: 425°F, Mold Temperature: 125°F)Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 1.4 %
1.4 %
(24 hr); ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D638
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Flexural Yield Strength 34.5 MPa
5000 psi
ASTM D790
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 4.11 J/cm
7.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
ASTM D648
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 218 °C
424 °F
Injection
Mold Temperature 52.0 °C
126 °F