| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Adell AR-18 Nylon 66, 40% Glass Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.47 g/cc | 0.0531 lb/in³ | ASTM D792 |
| Water Absorption | 0.60 % | 0.60 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 101 | 101 | ASTM D785 |
| Hardness, Rockwell R | 123 | 123 | ASTM D785 |
| Tensile Strength, Ultimate | 221 MPa | 32100 psi | ASTM D638 |
| Elongation at Break | 3.5 % | 3.5 % | ASTM D638 |
| Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
| Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
| Compressive Yield Strength | 276 MPa | 40000 psi | ASTM D695 |
| Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 263 °C | 505 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | >= 249 °C | >= 480 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | >= 249 °C | >= 480 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |