A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade
Manufacturer A. Schulman, Inc.
Trade Name POLYTROPE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature impact strength. TPP 504E is UV stable, paintable and pigmentable.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Melt Index of Compound 0.80 g/10 min
0.80 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength at Break 13.8 MPa
2000 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 0.310 GPa
45.0 ksi
ASTM D790
Gardner Impact 36.0 J

@Temperature -30.0 °C
26.6 ft-lb

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Brittleness Temperature -50.0 °C
-58.0 °F