Aclo Accutech Polypropylene Homopolymer HP0339C10L1 Calcium Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0339C10L1 Calcium Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
MD; ASTM D955
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Ash 10 %
10 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength at Break 11.0 MPa
1600 psi
ASTM D638
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 131 %
131 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 1.40 GPa
203 ksi
ASTM D638
Flexural Strength 37.0 MPa
5370 psi
ASTM D790
Flexural Modulus 1.500 GPa
217.5 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.9 °C
138 °F