Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 21 g/10 min @Load 3.80 kg, Temperature 230 °C |
21 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 51 KC General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 21 g/10 min @Load 3.80 kg, Temperature 230 °C |
21 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Polycasa Acryl® G 55 Acrylic, Injection Molding Grade Injection molding grade for very long flow paths, as well as thin-walled parts.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 190 °C |
21 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers Kepital® TC30-20 Description: Natural Acetal Copolymer, 10% Talc Reinforced GradeInformation provided by Network Polymers Inc. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 260 °C |
21 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® RCY6214 PC+ABS (Asia Pacific) Cycoloy* RCY6214 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1.5 mm. D.. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 230 °C |
21 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 2-2110 10% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2110 is a 10% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-2110 is developed for producing.. |
|||
Melt Flow | 21 g/10 min @Load 5.00 kg, Temperature 260 °C |
21 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® DP CF 2200 000000 PBT+PC PBT+PC, non-reinforced, injection molding, flame retardant, impact modified, low tendency to warp |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 230 °C |
21 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical LUPOL MC4352 PP+Rubber+MF Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9.. |
|||
Melt Flow | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 230 °C |
21 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7450 PP SABIC® PPcompound 7450 is a mineral filled, impact modified polypropylene TPO. This material can exhibit high impact resistance and good paintability in automotive exterior applications. The IMDS.. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 265 °C |
21 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Melt Flow | 21 g/10 min @Load 5.00 kg, Temperature 260 °C |
21 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 260 °C |
21 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL N802 PPE+HIPS (Asia Pacific) PPE/PS 80oC V2 FR high flow |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 190 °C |
21 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE DescriptionPOLYBATCH® Cedar 10310U is a cedar color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabi.. |
|||
Melt Flow | 21 g/10 min @Load 3.80 kg, Temperature 230 °C |
21 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
PlastxWorld CEVIAN® DR620 PC Alloy High impact, heat resistant, excellent moldability and indoor light stability.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information p.. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 230 °C |
21 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene DescriptionPolyfort® FPP 1876 is a 22% mineral filled copolymer UV Inhibited Polypropylene. It is high flow. Information provided by A. Schulman. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 190 °C |
21 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE DescriptionPOLYBATCH® Cedar 10310U is a cedar color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabi.. |
|||
Melt Flow | 21 g/10 min @Load 5.00 kg, Temperature 260 °C |
21 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Goodfellow TPX® MX002O Polymethylpentene This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi.. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 190 °C |
21 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Red 5500 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 5500 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5500 is heavy .. |
|||
Melt Flow | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
estimated from MVR using room temperature density; ISO 1133 |
Covestro Makrolon® GF8001* Polycarbonate, 20% Glass Filled ISO 7391-PC,MR,(,,)-18-3,GF20Developmental productFormerly Makrolon DP1-1951MVR (300 °C/1.2 kg) 16 cm3/10 min20 % Glass fiber reinforcedLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 230 °C |
21 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PP-HP20NS Homopolymer, 20 Melt Flow, Nucleated, Anti-stat This product is intended for general purpose injection molding applications such as cutlery, caps and closures, and thin-wall containers.Information provided by Entec |
|||
Melt Flow | 21 g/10 min @Load 5.00 kg, Temperature 260 °C |
21 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedPreprocessingMax. Water content |
|||
Melt Flow | 21 g/10 min | 21 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Homopolymer HP0339C10L Calcium Reinforced |
|||
Melt Flow | 21 g/10 min @Load 10.0 kg, Temperature 220 °C |
21 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Melt Flow | 21 g/10 min | 21 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Homopolymer HP0339T40L Talc Reinforced |
|||
Melt Flow | 21 - 27 g/10 min | 21 - 27 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX D5618 T RXF Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Melt Flow | 21 g/10 min @Load 10.0 kg, Temperature 220 °C |
21 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Melt Flow | 21 g/10 min | 21 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 6404 BLK Ash is 41%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 21 g/10 min | 21 g/10 min | ISO 1133 |
Solvay Engineered Polymers DEXFLEX® 900 TPO
(discontinued **) Description: DEXFLEX® 900 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paint.. |
|||
Melt Flow | 21 g/10 min @Load 2.16 kg, Temperature 230 °C |
21 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |