Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
Network Polymers NPP 50-0863
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
Huntsman Rexell® H2105 Injection Molding LLDPE  (discontinued **)
Linear-low high density, injection molding, FDA compliant.Features: High impact strength with reasonable flow.Applications: Articles that must withstand long-term heavy loading such as bottle crates..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Chevron Phillips HiD® 9605D HDPE Cast Film Resin  (discontinued **)
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Chevron Phillips HiD® 9607D HDPE Cast Film Resin  (discontinued **)
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D4883
Chevron Phillips HiD® 9720 HDPE Injection Molding Resin  (discontinued **)
Resin Type: linear homopolymerCharacteristics: good flow, moderate impact strength, excellent stiffness, moderate ESCR, moderate shrinkage resistanceApplications: pails, structural foamInformation p..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D792
NOVA Chemicals Sclair® 69A HDPE Extrusion Resin  (discontinued **)
Features: High tensile strength, better moisture barrier, better oil and solvent resistance, lower friction coefficient, lower brittleness temperature, better abrasion resistance, better temperature..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D 792
Total Finathene® 6450 HDPE film  (discontinued **)
Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin..
Density 0.962 - 1.54 g/cc
0.0348 - 0.0555 lb/in³
Average value: 1.29 g/cc Grade Count:107
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D 792
NOVA Chemicals Sclair® 99K Homopolymer HDPE Film Resin
99K complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te..
Density 0.962 g/cc
0.0348 lb/in³
Exxon Method
ExxonMobil Iotek® 7520 Zinc Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A "soft" zinc ionomer with excellent flexibility and impact strength. This ionomer has outstanding adhesion to glass, metals and paper. IOTEK iono..
Density 0.963 g/cc
0.0348 lb/in³
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade
Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats..
Density 0.964 g/cc
0.0348 lb/in³
ASTM D1505
ICO Polymers ICOFLOâ„¢ 510-5008 1200 Micron HDPE Powder
Description: ICOFLO 510-5008 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Global B-6200 High Density Polyethylene
Description-suitable for high quality blow molding, provides excellent surface glossiness in combination w/ outstanding environmental stress cracking resistanceApplications-cosmetics bottles, shampo..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Global J-2208 High Density Polyethylene
Description-industrial injection grade w/ UV stabilizer, good for high impact strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Global J-2308 High Density Polyethylene
Description-industrial injection grade w/ UV stabilizer, good for high impact strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided..
Density 0.964 g/cc
0.0348 lb/in³
JPJ Technologies 2200J HDPE Injection
Information provided by JPJ Technologies
Density 0.963 g/cc
0.0348 lb/in³
ISO 1183
Borealis BL2631 High Density Polyethylene
BL2631 is a high density polyethylene homopolymer intended for blow molding of products requiring high toughness and stiffness. Applications: fresh milk bottles, and juice bottles.Information provi..
Density 0.963 g/cc
0.0348 lb/in³
ISO 1872-2/ISO 1183
Borealis Borcell™ HE1123 High Density Polyethylene
Borcell™ HE1123 is a high density polyethylene compound intended for the insulation of radio frequency coaxial cables. Borcell™ HE1123 is designed to give the lowest possible cable attenuation by..
Density 0.962 g/cc
0.0348 lb/in³
ISO 1183
Borealis CG9620 High Density Polyethylene
CG9620 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Applications: CG9620 is recommended for coated film and co-extrusion..
Density 0.964 g/cc
0.0348 lb/in³
ISO 1183
Borealis MG9641B Polyethylene
MG9641B is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
Density 0.964 g/cc
0.0348 lb/in³
ASTM D1505
Chevron Phillips Marlex® EHM 6007 High Density Polyethylene
High Density PolyethyleneCustomer Benefits: A blow molding grade rein that offers a high quality product for those critical food packaging jobs and good impact strength and stiffness.Applications: L..
Density 0.964 g/cc
0.0348 lb/in³
ASTM D4883
ExxonMobil HDPE HMA 025 High Density Polyethylene Resin
Product Description: HMA 025 is a HDPE grade, characterized by excellent dimensional stability, impact strength and very high stiffness. Availability: Africa & Middle East, Asia Pacific and Europe A..
Density 0.963 g/cc
0.0348 lb/in³
Dow HDPE 05862N High Density Polyethylene
Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
Density 0.962 g/cc
0.0348 lb/in³
Dow HDPE 10462N High Density Polyethylene
DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability..
Density 0.964 g/cc
0.0348 lb/in³
ASTM D1505
Chevron Phillips Marlex® K607 High Density Polyethylene  (discontinued **)
High Density PolyethyleneCustomer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.Applications: Recommended resin for thin sheet, cut sheet up to..
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Chevron Phillips Marlex® HMN 6060 Polyethylene, Injection Molding Grade, HDPE  (discontinued **)
Meets FDA Regulation 177.1520.Data provided by the manufacturer
Density 0.965 g/cc
0.0348 lb/in³
Mixed
ITW Plexus Plexus™ MA925 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works.
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
ExxonMobil Paxon™ 4700 Blown Film Extrusion Resin  (discontinued **)
4700 is a medium molecular weight, high density polyethylene homopolymer film resin. It can be processed on conventional film extrusion equipment.Information provided by ExxonMobil Chemical
Density 0.963 g/cc
0.0348 lb/in³
ISO 1183
Unipetrol PE HD LITEN® MB/ML 71 HDPE
Made for injection molding applications.Information provided by Unipetrol RPA
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Chevron Phillips MarFlex® 9608XD HDPE Film Grade
This HDPE is tailored for applications that require:Very low gel levelsVery "clear" filmExcellent drawdownEnhanced stiffnessExcellent WVTR for a chill cast filmExcellent ProcessibilityTypical Cast F..