Aclo Accutech Polypropylene Homopolymer HP0334M40L Mica Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Mica Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0334M40L Mica Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
MD; ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
ASTM D785
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 3.900 GPa
565.6 ksi
ASTM D638
Flexural Strength 42.0 MPa
6090 psi
ASTM D790
Flexural Modulus 4.200 GPa
609.1 ksi
ASTM D790
Izod Impact, Notched 0.422 J/cm
0.790 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
252 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.2 °C
171 °F