Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Chemlam® RL® RL5000 PTFE-Coated Non-woven Aramid Reinforced Laminate

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Chemlam® RL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Chemlam® RL® RL5000 PTFE-Coated Non-woven Aramid Reinforced Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sintered PTFE for low friction, flame resistance, chemical and barrier properties. Chemlam® RL® series is a high performance composite that has desirable elongation properties, and is easy to fabricate using standard techniques such as sewing for conversion to finished articles.RL 5000 Reinforcement: Non-woven Aramid. All data based on a 0.0185 inch test sample. Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 0.758 g/cc
0.758 g/cc
Woven Density
Mechanical Properties Metric English Comments
Tear Strength 4.38 kN/m
25.0 pli
Fill/Transverse direction
8.77 kN/m
50.0 pli
Warp/Longitudinal direction
Descriptive Properties Value Comments
Color Orange/White
Weight (oz/yd^2) 10.5
Copyright © lookpolymers.com All Rights Reserved