Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROLENE® ARPE LD 300-1 LDPE Black Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Sheet/Profile extrusions
Manufacturer Aaron Industries Corporation
Trade Name AAROLENE® ARPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROLENE® ARPE LD 300-1 LDPE Black Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AAROLENE® ARPE 300 Series Polyethylene Compounded Resin, LDPE BlackFeatures: A compounded LDPE, black, low melt resin specifically designed for all profile extrusion applications.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 11.0 MPa
1600 psi
ASTM D638
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ASTM D648