Material Notes:
Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-10All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 40
40
Apparent
Tensile Strength, Ultimate 124 MPa
18000 psi
Tensile Strength, Yield 89.6 MPa
13000 psi
Elongation at Break 2.0 %
2.0 %
given as inch/inch in one inch gauge length
Modulus of Elasticity 96.5 GPa
14000 ksi
Flexural Strength 248 MPa
36000 psi
Transverse Rupture
Charpy Impact, Unnotched 4.07 J
3.00 ft-lb