PRODUCT NO. Category Trade Name
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled TISAKRIL®
Tisan TISAKRIL® Flame Retardant (V0) ABS Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant TISAKRIL®
Tisan TISAKRIL® UNR ABS ABS Polymer TISAKRIL®
Tisan TISAPET® 20% Glass Reinforced Polyethylene Terephthalate Polyethylene Terephthalate (PET), 20% Glass Reinforced TISAPET®
Tisan TISAPET® 30% Glass Reinforced Polyethylene Terephthalate Polyethylene Terephthalate (PET), 30% Glass Reinforced TISAPET®
Tisan TISAPET® UNR Polyethylene Terephthalate Polyethylene Terephthalate (PET) TISAPET®
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate Polycarbonate, 10% Glass Filled TISARBON®
Tisan TISARBON® Flame Retardant (V0) Polycarbonate Polycarbonate, Unreinforced, Flame Retardant TISARBON®
Tisan TISARBON® UNR Polycarbonate Polycarbonate (PC) TISARBON®
Tisan TISBLEND® PC/ABS Polycarbonate/ABS Alloy, Unreinforced TISBLEND®
Tisan TISESTER® 15% Glass Fiber Reinforced and Heat Stabilized Polybutylene Terephthalate Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled TISESTER®
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled TISESTER®
Tisan TISESTER® 30% Glass Fiber Reinforced and heat Stabilized Polybutylene Terephthalate Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled TISESTER®
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled TISESTER®
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant TISESTER®
Tisan TISESTER® 30% Glass Fiber Reinforced, Impact Resistance and Heat Stabilized ISI Stab. Polybutylene Terephthalate Polybutylene Terephthalate (PBT), Impact Grade TISESTER®
Tisan TISESTER® Flame Retardant (V0). Heat Stabilized Polybutylene Terephthalate Polybutylene Terephthalate (PBT), Flame Retardant TISESTER®
Tisan TISESTER® UNR Polybutylene Terephthalate Polybutylene Terephthalate (PBT), Unreinforced, Molded TISESTER®
Tisan TISETILEN® Flame Retardant (V0) Polyethylene HDPE TISETILEN®
Tisan TISETILEN® UNR Polyethylene LDPE TISETILEN®
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6 Nylon 6, 20% Glass Fiber Filled TISLAMID®
Tisan TISLAMID® 6 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 6 Nylon 6, Glass/Mineral Reinforced TISLAMID®
Tisan TISLAMID® 6 20% Glass Fiber Reinforced, Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6 Nylon 6, Glass Fiber Filled, Flame Retardant TISLAMID®
Tisan TISLAMID® 6 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 6 Nylon 6, Glass Fiber Filled, Flame Retardant TISLAMID®
Tisan TISLAMID® 6 30% Glass Bead Reinforced Nylon 6 Nylon 6, Glass Bead Filled TISLAMID®
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 Nylon 6, 30% Glass Fiber Filled TISLAMID®
Tisan TISLAMID® 6 30% Glass Filled Impact Modified Nylon 6 Nylon 6, Glass Filled, Impact Grade TISLAMID®
Tisan TISLAMID® 6 30% Glass Filled Impact Modified, Heat Stabilized Nylon 6 Nylon 6, 30% Glass Fiber Filled TISLAMID®
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6 Nylon 6, 30% Mineral Filled TISLAMID®
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6 Nylon 6, Unreinforced, Flame Retardant TISLAMID®
Tisan TISLAMID® 6 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6 Nylon 6, Unreinforced, Flame Retardant TISLAMID®
Tisan TISLAMID® 6 UNR Nylon 6 Nylon 6, Unreinforced TISLAMID®
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66 Nylon 66, 10% Glass Fiber Filled TISLAMID®
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66 Nylon 66, Heat Stabilized TISLAMID®
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66 Nylon 66, 20% Glass Fiber Filled TISLAMID®
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 Nylon 66, Glass Fiber Filled, Flame Retardant TISLAMID®
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 Nylon 66, Glass Fiber Filled, Flame Retardant TISLAMID®
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66 Nylon 66, 30% Glass Fiber Filled TISLAMID®
Tisan TISLAMID® 66 30% Glass Bead Reinforced Nylon 66 Nylon 66, Glass Bead Filled TISLAMID®
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66 Nylon 66, 30% Glass Fiber Filled TISLAMID®
Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66 Nylon 66, Glass Reinforced, Impact Grade TISLAMID®
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66 Nylon 66, 30% Mineral Filled TISLAMID®
Tisan TISLAMID® 66 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 66 Nylon 66, Unreinforced, Flame Retardant TISLAMID®
Tisan TISLAMID® 66 Flame Retardant (V0). Heat Stabilized Nylon 66 Nylon 66, Unreinforced, Flame Retardant TISLAMID®
Tisan TISLAMID® 66 Impact Modified Nylon 66 Nylon 66, Impact Grade TISLAMID®
Tisan TISLAMID® 66 UNR Nylon 66 Nylon 66, Unreinforced TISLAMID®
Tisan TISMOSET® Thermoset TISMOSET®
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene Polypropylene with 10% Calcium Carbonate (CaCO3) Filler TISOPLEN®
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Homopolymer Polypropylene Polypropylene with 10% Calcium Carbonate (CaCO3) Filler TISOPLEN®
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Copolymer Polypropylene Polypropylene with 10% Talc Filler TISOPLEN®
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Homopolymer Polypropylene Polypropylene with 10% Talc Filler TISOPLEN®
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene Polypropylene, Flame Retardant TISOPLEN®
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene Polypropylene, Flame Retardant TISOPLEN®
Tisan TISOPLEN® 30% Glass Fiber Filled Reinforced Heat Stabilized Homopolymer Polypropylene Polypropylene with 30% Glass Fiber Filler TISOPLEN®
Tisan TISOPLEN® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polypropylene Polypropylene with 30% Glass Fiber Filler TISOPLEN®
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Copolymer Polypropylene Polypropylene with 30% Talc Filler TISOPLEN®
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Homopolymer Polypropylene Polypropylene with 30% Talc Filler TISOPLEN®
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene Polypropylene with 40% Calcium Carbonate (CaCO3) Filler TISOPLEN®
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene Polypropylene with 40% Calcium Carbonate (CaCO3) Filler TISOPLEN®
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Copolymer Polypropylene Polypropylene with 40% Talc Filler TISOPLEN®
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Homopolymer Polypropylene Polypropylene with 40% Talc Filler TISOPLEN®
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene Polypropylene, Flame Retardant TISOPLEN®
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene Polypropylene, Flame Retardant TISOPLEN®
Tisan TISREN® Flame Retardant (V0) Polystyrene Polystyrene, Flame Retardant TISREN®
Tisan TISSAN® Flame Retardant (V0) Styrene Acrylonitrile SAN Polymer TISSAN®
Tisan TISSAN® UNR Styrene Acrylonitrile SAN Polymer TISSAN®
Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Copolymer Polypropylene Polypropylene with 20% Calcium Carbonate (CaCO3) Filler TISOPLEN®
Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Homopolymer Polypropylene Polypropylene with 20% Calcium Carbonate (CaCO3) Filler TISOPLEN®
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Copolymer Polypropylene Polypropylene with 20% Talc Filler TISOPLEN®
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene Polypropylene with 30% Calcium Carbonate (CaCO3) Filler TISOPLEN®
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Homopolymer Polypropylene Polypropylene with 30% Calcium Carbonate (CaCO3) Filler TISOPLEN®
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Homopolymer Polypropylene Polypropylene with 20% Talc Filler TISOPLEN®
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene Polypropylene, Flame Retardant TISOPLEN®
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Polypropylene Polypropylene, Flame Retardant TISOPLEN®
Tisan TISAKRIL® 30% Glass Fiber Reinforced ABS Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled TISAKRIL®