Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data) Duratron U1000 PEI is an amber translucent (non-optical quality) amorphous thermoplastic material, offering high strength and heat resistance. It performs continuously to 170 °C, making it ideal fo.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data) Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data) Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data) Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat agein.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data) Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data) TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data) Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
Volume Resistivity | 1.0e+14 - 1.0e+16 ohm-cm | 1.0e+14 - 1.0e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Volume Resistivity | 1.0e+14 - 1.0e+16 ohm-cm | 1.0e+14 - 1.0e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Volume Resistivity | 1.0e+14 ohm-cm | 1.0e+14 ohm-cm | ASTM D257 |
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM) Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data) This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural.. |