Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+7 ohm-cm | >= 1.00e+7 ohm-cm | ASTM D257 |
Polikim EFALON® B-60 PTFE, 60% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 93 |
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite Properties:Good thermal conductivityLow coefficient of frictionLow permeabilityApplications: Non-lubricated dynamic seals.Information provided by Isoflon. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 CF20 L 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Semi Conductive and LubricatedInformation provided by TP C.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC CF20 CR X 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Good Chemical Resistance and Semi ConductiveInformation provided by TP Compos.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC/PET CF20 IM 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact Modified and Semi ConductiveAppearance: Black.. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+11 ohm-cm | 1.00e+7 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0164 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PEI CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Lubrizol Hipscon™ M-505 Static Control High Impact Polystyrene Hipscon™ M-505 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unifo.. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+11 ohm-cm | 1.00e+7 - 1.00e+11 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW300 (COND) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW341 (COND) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1e+05 - 1.00e+7 ohm-cm | 1e+05 - 1.00e+7 ohm-cm | |
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Volume Resistivity | 1e+05 - 1.00e+7 ohm-cm | 1e+05 - 1.00e+7 ohm-cm | ASTM D257 |
Clariant Renol PPSP0017 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 805 PTFE, 40% Bronze Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 807 PTFE, 40% Bronze + 5 MoS2 Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 812 PTFE, 46% Bronze, Green Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 817 PTFE, 60% Bronze Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PPS GF35 SS7 BK 35/7% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel Fiber, 35/7% Filler by WeightUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
Arkema Group Pebax® MV 2080 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 2080 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 2080 is an inherently dissipative polymer and can be dry blended or compounded w.. |
|||
Volume Resistivity | <= 1.00e+7 ohm-cm | <= 1.00e+7 ohm-cm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PA 1408 Conductive Thermoplastic Compound PRE-ELEC® PA 1408 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | 1V; IEC 60093 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |