Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
Manufacturer Isoflon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Properties:Good thermal conductivityLow coefficient of frictionLow permeabilityApplications: Non-lubricated dynamic seals.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 2.14 - 2.19 g/cc
2.14 - 2.19 g/cc
ASTM D792
Deformation 5.0 - 6.0 %

@Time 86400 sec
5.0 - 6.0 %

@Time 24.0 hour
Permanent, after Relaxation; ASTM D695
10 - 12 %

@Time 86400 sec,
Pressure 13.7 MPa
10 - 12 %

@Time 24.0 hour,
Pressure 1990 psi
Under Load; ASTM D695
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 60
55 - 60
ASTM D2240
Tensile Strength 18.0 - 23.0 MPa
2610 - 3340 psi
ASTM D4894
Elongation at Break 200 - 250 %
200 - 250 %
ASTM D4894
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
ASTM D257
Descriptive Properties Value Comments
Ageing and Weatherability Stable over 20 years of exposure