Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Quantum Composites LYTEX® 4084 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4084 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-20Txx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape
(discontinued **) Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | NBR 5403 |
Karina E MCP 520 Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | ASTM D 257 |
Karina Karintox 70 Polyolefin Compound Halogen free, fire retardant, low smoke and fume polyolefinic compound. Recommended for insulation of electrical cables up to 1KV.Information provided by Karina Indústria e Comércio de Plá.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | |
Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | ASTM D 257 |
Karina E 105440-35/1-Y-IS-SD-LM Ivory PVC Compound Heavy metal free PVC compound, recommended for thin wall insulation of automotive electrical wires for working at the temperature range of -40°C to 105°CInformation provided by Karina Indús.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | NBR 5403 |
Karina 70900-35/1-E-AC Ivory PVC Compound Flame retardant PVC compound, class 70C (PVC/A), recommended for insulation of electrical wires and cables (BWF).Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF/M15 A1 BK 15% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 15% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized Appearance: BlackInformation provided by TP Compo.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF10 TL10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedApp.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF10 TL10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated and Heat Stabiliz.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF6 HS BK 6% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance:.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF7 L 7% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 7% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF8 IM4 HS L 8% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Compo.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | |
Master Bond MasterSil 708FR One Part, Flame Resistant Silicone Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of .. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | IEC 60093 |
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | IEC 60093 |
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | E24/125; IPC TM-650 2.5.17.1 |
Arlon 84N Polyimide Laminate and Prepreg 84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-05Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-07Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon LW201Xxx-M1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Mylar Interleave Design/Construction:Cross Section Type: TriangularArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for subsequent.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-15Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 940-10Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Teknor Apex APEX® 80851-B Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Forms: Pellets Uses: Wire and Cable Applications Wire Types: THW; TW; THHN; THWN Agency Ratings: UL QMTT2 .E73402Information Provided by Teknor Apex |
|||
Volume Resistivity | 3.00e+14 ohm-cm @Temperature 20.0 °C |
3.00e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Fainplast Compounds HAX HF 28 Halogen Free PVC Sheathing; good mechanical properties |