Material Notes:
Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of 0.75 mm and 94V.0 for a 3 mm thickness. It adheres well to a wide variety of substrates including glass, metals and many plastics. The rapidity of the cure depends on the thickness of the layer and the humidity; the thicker the layer the slower the cure. It is exceptionally soft with good elasticity and flexibility, and outstanding electrical insulation properties. Most importantly, it is non-corrosive, fast setting, and has a flowable consistency. MasterSil 708FR is serviceable over the broad temperature range of -45°C to +200°C, as per UL specifications, and is gray in color.Information provided by MasterBond®
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Viscosity 25000 - 45000 cP
25000 - 45000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 30 - 40
30 - 40
Tensile Strength at Break 2.07 - 2.76 MPa
300 - 400 psi
Elongation at Break 200 - 300 %
200 - 300 %
Shear Strength 1.03 - 1.38 MPa
150 - 200 psi
Tensile, Al to Al
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -42.8 °C
-45.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+14 ohm-cm
3.00e+14 ohm-cm
Dielectric Constant 3.2

@Frequency 60.0 Hz,
Temperature 25.0 °C
3.2

@Frequency 60.0 Hz,
Temperature 77.0 °F
Dielectric Strength 23.6 kV/mm

@Thickness 3.17 mm
600 kV/in

@Thickness 0.125 in
Dissipation Factor 0.010

@Frequency 60.0 Hz,
Temperature 25.0 °C
0.010

@Frequency 60.0 Hz,
Temperature 77.0 °F
Processing Properties Metric English Comments
Cure Time 10.0 - 15.0 min
0.167 - 0.250 hour
Tack-free time
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers
Descriptive Properties Value Comments
Appearance gray