Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex APEX® 80851-B Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 80851-B Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: 105°C Insulation; RoHS Compliant Forms: Pellets Uses: Wire and Cable Applications Wire Types: THW; TW; THHN; THWN Agency Ratings: UL QMTT2 .E73402Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 71
71
10 seconds; ASTM D2240
Tensile Strength at Break 22.8 MPa
3300 psi
ASTM D638
Elongation at Break 330 %
330 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -33.0 °C
-27.4 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+14 ohm-cm
3.00e+14 ohm-cm
ASTM D257
Dielectric Constant 3.01

@Frequency 1.00e+6 Hz
3.01

@Frequency 1.00e+6 Hz
ASTM D150
4.26

@Frequency 1000 Hz
4.26

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.053

@Frequency 1.00e+6 Hz
0.053

@Frequency 1.00e+6 Hz
ASTM D150
0.076

@Frequency 1000 Hz
0.076

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: