Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1200-03 Polycarbonate Resin Description: LUPOY PC 1200-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1200-08 Polycarbonate Resin Description: LUPOY PC 1200-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1201-15 Polycarbonate Resin Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1301-10 Polycarbonate Resin Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1301EP30 Polycarbonate Resin Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 3030-15 Polycarbonate Resin Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1300-03 Polycarbonate Resin Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1302EP-30 Polycarbonate Resin Description: LUPOY PC 1302EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron EMERGEâ„¢ 4330-22 Polycarbonate EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. .. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 302V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity (for tinted/transparent colors), and is available in both tint.. |
|||
Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
Styron EMERGEâ„¢ 4330-6 Polycarbonate EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information .. |