Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
PolyOne Geon™ Vinyl Wire & Cable 1741-xx06D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257-99 |
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257-99 |
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | 80°C for 1,000 hrs; JIS-K-6249; ASTM D 257 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | |
Saint-Gobain Korel® K30-15 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D247 |
Plenco 6015 Phenolic, Briquette, Transfer Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
Tipco Tipcolite® THD 111 Phenolic Compound, Short Glass Fibers & Minerals, Medium -Soft Flow & High Strength Medium -Soft Flow Phenolic Compound, Reinforced with Short Glass Fibres & MineralsApplications: Automotives & ElectricalProcessing: Compression & TransferInformation provided by the Manufacturer, T.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ P40H Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ P40H-05 Polyester TPE, Non-smell, Non-deposit Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ P40U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ S1002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | |
Dow Corning FLUOROGEL® Q3-6679 DIELECTRIC GEL KIT Two-part, clear, RT or heat cure, solvent and fuel resistant.Information provided by Dow Corning |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | IEC 60093 |
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | IEC 60093 |
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Volume Resistivity | >= 2.00e+12 ohm-cm | >= 2.00e+12 ohm-cm | |
Epoxy Technology EPO-TEK® 301-2 Optically Transparent Epoxy Product Description: EPO-TEK® 301-2 is a two component optical, medical, and semiconductor grade epoxy resin, with low viscosity, long pot-life, and good handling characteristics.Advantages & Appli.. |
|||
Volume Resistivity | >= 2.00e+12 ohm-cm | >= 2.00e+12 ohm-cm | |
Epoxy Technology EPO-TEK® OD2002 High Temperature Epoxy Material Description: High Tg version of EPO-TEK®353ND with low modulus and good toughness. Replacement for EPO-TEK® 364. Complies with USP Class VI biocompatibility standards.Information Provid.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | |
Saint-Gobain Korel® K30-20 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |
|||
Volume Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | |
Saint-Gobain Korel® K30-25 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |