Saint-Gobain Korel® K30-25 Soft Micro-cellular Polyurethane Foam

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Korel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Korel® K30-25 Soft Micro-cellular Polyurethane Foam.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microcellular foams are categorized by degree of deflection force. By varying the modulus and density, Saint Gobain Performance Plastics has developed this series of materials that meets the demands of design engineers today. All Korel fians are available with an aggressive acrylic adhesive on one side to facilitate placement. Korel K30 foams are soft, conformable, low deflection, urethane foams offering excellent compression set resistance and low out-gassing that exceeds fogging requirements. K30 is ideal for open/close applications.FEATURES/BENEFITS:Excellent compression set resistanceHighly resilient (will not collapse)Dissipates stressesResistant to moisture and most chemicalsConformable and flexible even in extreme environmental conditionsEasy to achieve intricate die-cut partsAggressive acrylic adhesive (optional) facilitates assemblyAvailable cast on to polyester film for stability and low deformationTypical Applications: Cellular telephones, electrical enclosures, electronic gasketing, vibration damping, cushioning, acoustical control, bumpers, instrument panels, spacers.Specification Notes: Passes Fogging Test SAE-J 1756, 3 hrs. at 212°F (100°C). All data based on a 0.045 inch test sample.(Available in multiple thicknesses.) Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 0.401 g/cc
0.0145 lb/in³
ASTM D1667
Water Absorption 15 %
15 %
% by weight; ASTM D3574
Mechanical Properties Metric English Comments
Hardness, Shore O 20
20
ASTM D2240
Tensile Strength, Yield 0.689 MPa
100 psi
ASTM D3574
Elongation at Break 340 %
340 %
ASTM D3574
Tensile Modulus 0.000276 GPa
0.0400 ksi
ASTM D3574
Compressive Strength 0.0414 MPa
6.00 psi
Compression Deflection, Value given for 12.7 mm/min, 25% deflection.; ASTM D3574 Test C
Compressive Modulus 0.0000552 GPa
0.00800 ksi
Force to Compress, Value given for 25% compression; ASTM D1667
Tear Strength 2.63 kN/m
15.0 pli
Initial Tear Strength; ASTM D624 Die C
Compression Set <= 3.0 %
<= 3.0 %
Constant Deflection at 73°F; ASTM D 3574 Test D
<= 7.0 %

@Temperature 70.0 °C
<= 7.0 %

@Temperature 158 °F
Constant Deflection; ASTM D 3574 Test D
Thermal Properties Metric English Comments
Thermal Conductivity 0.0865 W/m-K
0.600 BTU-in/hr-ft²-°F
ASTM E1530
Maximum Service Temperature, Air 70.0 °C
158 °F
Constant use
121 °C
250 °F
Intermittent
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+12 ohm-cm
2.00e+12 ohm-cm
Surface Resistivity per Square 9.10e+13 ohm
9.10e+13 ohm
Dielectric Strength 1.89 kV/mm
48.0 kV/in
ASTM D149
Descriptive Properties Value Comments
Standard Color Black