Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 33.0 kV/mm | 838 kV/in | |
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | STN IEC 60243 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | VDE 0303 |
GEHR Plastics PEI Polyetherimide Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and creep resistance. Its unique torque strength permits the economic.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | IEC 60243-1 |
Lanxess Durethan® DP BKV 60 H2.0 EF 900116 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, low viscosity, good flowability (Easy Flow), good heat-resistanceApplication Examples: gearbox housings, spring holders, automotive door handles |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | ASTM D149 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | IEC 60250 |
Polyram RamTough PZ126 Polycarbonate, Low Viscosity General purpose, low viscosity polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 33.0 kV/mm @Thickness 1.00 mm |
838 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Unitika CX-2500 PA6, Dry Transparent nylonInformation provided by Unitika Ltd. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | cond; IEC 60243-1 |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-2 FWA nat PA*-GF20 Product description: Grivory GV-2 FWA natural is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyami.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40 Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-5H black PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60 Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GVL-5H nat PA*-GF50 Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® HT XE 3996 PA*-GF30 Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designatio.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30 Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50 Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PA 12 Nylon 12 Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorptio.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | 50%RH; IEC 60243-1 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | IEC 60243-1 |
DSM Arnite® AV2 370 XT PET-GF35 35% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60 Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | DAM; IEC 60243-1 |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | CEI 60243-1 |
Addiplast Addinyl B2 V20 Nylon 6. 20% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | IEC 60243-1 |
Lanxess Pocan® DP T 7140 LDS 000000 PBT + PET, 44% Mineral + L227Glass Fiber
(discontinued **) PET+PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimension stability |