Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D149 |
Quantum Composites LYTEX® 4084 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4084 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 3.17 mm |
500 kV/in @Thickness 0.125 in |
|
Ineos Nova 602 Crystal Polystyrene GP Grade
(discontinued **) Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
Arkema Group Oroglas® MI-2T Acrylic
(discontinued **) OROGLAS MI-2T is an injection molding acrylic grade that offers excellent thermal resistance with slight improvement in impact performance.Key features improved deformation and toughness : up to 2.. |
|||
Dielectric Strength | 19.7 - 24.0 kV/mm | 500 - 610 kV/in | Average value: 21.1 kV/mm Grade Count:3 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Dielectric Strength | 19.7 - 43.0 kV/mm | 500 - 1090 kV/in | Average value: 31.2 kV/mm Grade Count:24 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 3.17 mm |
500 kV/in @Thickness 0.125 in |
|
Ineos Nova 1290 High Heat Crystal Polystyrene Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D1490 |
Lord Adhesives Thermosetâ„¢ EP-809 Ignition Coil Impregnating and Encapsulation Epoxy Lord EP-809 is a long working life, heat curing, two component epoxy formulation. It was designed especially for potting high voltage automotive ignition coils. The combination of low viscosity, exc.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® ASA GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
Saint-Gobain COHRlastic® CF3320 Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6 TS15 BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Silicone Lubricant and PTFE LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composite.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6/6 GF30 TS15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PPS GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D 696 |
Styrolution PS 1600 GPPS Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D 696 |
Styrolution PS 1900 GPPS Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D 696 |
Styrolution PS 2610 GPPS Extruded packaging; Thermoforming applicationsExcellent toughnessHigh melt strengthGood flow and processabilityInformation provided by Styrolution |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® ABS TX15 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
Saint-Gobain COHRlastic® CF4050 General Purpose Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
Dow Corning SE 738 SILICONE RTV One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB.Information provided by Dow Corning |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
Cotronics Bond-It™ 7040 Epoxy, Room Temperature Cure Forms high strength bonds to difficult metals, plastics, glass, ceramics, composites, etc. Cures at room temperature with high temperature strength and good electrical and thermal shock resistance... |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D149 |
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
Arkema Group Oroglas® VM Acrylic, Injection Molding Grade
(discontinued **) OROGLAS VM is an injection molding grade with a medium heat resistance and easy flow.OROGLAS VM is particularly suitable to improve mold filling of technical parts.The VM L version has been speciall.. |
|||
Dielectric Strength | 19.7 kV/mm | 500 kV/in | |
Chesterton 860 Moldable Polymer Gasketing Description: Chesterton® 860 Moldable Polymer Gasketing is a solid flexible gasketing material which fills in surface irregularities, stop leaks and never sticks to surfaces after curing. It is the.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 3.17 mm |
500 kV/in @Thickness 0.125 in |
|
Ineos Nova 4501 Medium Impact Polystyrene
(discontinued **) Good toughnessApplications: Light louvers, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provide.. |
|||
Dielectric Strength | >= 19.7 kV/mm | >= 500 kV/in | At 50 mils; ASTM D149 |
Borealis Borstar® HE6062 HDPE Black Jacketing Compound Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketin.. |