Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 330 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 13.0 - 19.0 kV/mm
330 - 483 kV/in
ASTM D149
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Dielectric Strength 13.0 kV/mm
330 kV/in
Short Time; Dry; ASTM D149
Resinoid 1363 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Dielectric Strength 13.0 kV/mm
330 kV/in
Short Time; Dry; ASTM D149
Resinoid 1365 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Dielectric Strength 13.0 kV/mm

@Thickness 3.20 mm
330 kV/in

@Thickness 0.126 in
Short-Time 500 V/sec
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Dielectric Strength 13.0 kV/mm
330 kV/in
ASTM D149
Plenco 5440 Black General Purpose Phenolic Molding Compound  (discontinued **)
Plaslok 5440 is the replacement material for the former Union Carbide BMRS-5440. It is a two-stage, phenolic molding compound that has been successfully formulated to accommodate a very wide range ..
Dielectric Strength 13.0 kV/mm
330 kV/in
ASTM D149
Plenco 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 501 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in heat resistant and electrical applications. It is designed for elevated temperature exposure for e..
Dielectric Strength 13.0 kV/mm
330 kV/in
150°C for 1,000 hrs
Fujipoly Industries Sarcon® 45U Thin-Film UR
Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
Dielectric Strength 13.0 kV/mm
330 kV/in
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 45U Thin-Film UR
Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
Dielectric Strength 13.0 kV/mm
330 kV/in
150°C for 1,000 hrs; JIS-K-6249
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b..
Dielectric Strength 13.0 kV/mm

@Thickness 1.59 mm
330 kV/in

@Thickness 0.0625 in
Perpendicular, Short Time in Oil and Air; ASTM D149
Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1)
This IEEE Class F 155ºC high strength material exhibits substantial resistance to cold flow or creep under heat and pressure. Suggested applications include motor slot wedges, washers, brush plat..
Dielectric Strength 13.0 kV/mm

@Thickness 3.00 mm
330 kV/in

@Thickness 0.118 in
ASTM D149
Teknor Apex Beetle® MD21 Nylon 6, Extrusion Grade
Notes: MD21 is a medium viscosity grade of nylon 6, designed for wire coating extrusion. MD21 is heavily pigment and is designed to provide good opacity even with thin coatings. It also features a..
Dielectric Strength 13.0 kV/mm
330 kV/in
Wet, short term. ASTM D149
Sumitomo Bakelite North America 4064 Mineral Filled Electrical Encapsulation Grade Epoxy
Rogers electrical encapsulation grade epoxy is recommended for capacitors, resistors, gold lead encapsulation, relays, coils and bobbins.Information provided by Sumitomo Bak North America, Inc.
Dielectric Strength 13.0 kV/mm
330 kV/in
AC
Sapco C 220 Steatite
Information provided by Sapco.
Dielectric Strength 13.0 kV/mm
330 kV/in
Short Time; ASTM D149
Plenco 1586 Polyester, Pellet, Injection Molded
PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti..
Dielectric Strength 13.0 kV/mm
330 kV/in
Wet, Step by Step
Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Dielectric Strength 13.0 kV/mm
330 kV/in
ASTM D149
Toyobo TS301 PPS, 30% Glass Fiber Reinforced
Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo..
Dielectric Strength 13.0 kV/mm
330 kV/in
ASTM D149-95a
Thermoseal KLINGERSIL® C-4324 Compressed Inorganic Fiber Gasketing
Recycled Fiberglass & Aramid BlendNitrile BinderLow Pressure Steam, Water & GasesGood for Oils and FuelsInformation provided by Thermoseal Inc.
Dielectric Strength 13.0 kV/mm
330 kV/in
Wet, Step by Step
Cosmic Plastics E4905 Mineral Filled Epoxy Molding Compound, Encapsulated Grade
Data provided by the manufacturer.
Dielectric Strength 13.0 kV/mm
330 kV/in
Dow Corning SE 4440 LP KIT
Two-part, grey, 1:1, addition cure gel, good thermal conductivity, low viscosity.Information provided by Dow Corning
Dielectric Strength 13.0 kV/mm
330 kV/in
ASTM D149
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience ..
Dielectric Strength 13.0 kV/mm
330 kV/in
ASTM D149
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 55 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience ..
Dielectric Strength 13.0 kV/mm
330 kV/in
DIN 53481
DSM Fibre Intermediates Nyrim® 2000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Dielectric Strength 13.0 kV/mm
330 kV/in
DIN 53481
Brueggemann Chemical Nyrim® 1000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Dielectric Strength 13.0 kV/mm
330 kV/in
Short Time
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester
BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium..
Dielectric Strength 13.0 kV/mm

@Thickness 2.00 mm
330 kV/in

@Thickness 0.0787 in
IEC 243-1
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Copyright © lookpolymers.com All Rights Reserved