Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 9.84 kV/mm | 250 kV/in | ASTM D149 |
Owens Corning Glass Fiber Reinforced Polyester (Spray-up/Lay-up), 30 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Permabond 738 Cyanoacrylate, toughened PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over.. |
|||
Dielectric Strength | 9.84 - 303 kV/mm | 250 - 7700 kV/in | Average value: 25.4 kV/mm Grade Count:105 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Permabond 200 Cyanoacrylate, wire tacking PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Permabond 260 Cyanoacrylate PERMABOND 260 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 260 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Permabond 265 Cyanoacrylate PERMABOND 265 is a medium viscosity cyanoacrylate ideal for intermediate gap fill application. PERMABOND 265 provides faster set times and improved gap-filling capability compared to conventional cy.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Permabond 798 Cyanoacrylate, Surface insensitive PERMABOND 798 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, Metals, Ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Dielectric Strength | 9.84 - 120 kV/mm | 250 - 3050 kV/in | Average value: 31.2 kV/mm Grade Count:101 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
GrafTech GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing GRAFOIL® Grade UCAR®-323 is a laminated gasket material consisting of multiple plies of woven fiberglass coated with PTFE. It will not support combustion or bacteria. Its applications include:.. |
|||
Dielectric Strength | 9.84 kV/mm @Thickness 3.00 mm |
250 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | Step by Step; ASTM D149 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Compression Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | Step by Step; ASTM D149 |
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Compression Grade Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | Step by Step; ASTM D149 |
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Injection Grade Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Cotronics Resbond™ 903HP High Temperature Ceramic Adhesive, Hi-Bond Strength |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Cotronics Resbond™ 904 Ultra Temp Zirconia Adhesive and Coating Ultra Temp 904 is a smooth creamy paste that is easily brushed on ceramics, graphite, metals, etc. to form adhesive bonds and coatings that will withstand 4000°F (2200°C) continuous heat. It has .. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Cotronics Resbond™ 906 High Temperature Ceramic Adhesive, High Expansion |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | ASTM D149 |
Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber (Ferromagnetic Filler) Substrate: Style 7628 Fiberglass This data represents typical value.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia Castable ceramic with high dielectric and physical strength. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Trelleborg Emerson & Cuming Stycast® 4640-25 Two-Component Silicone Flexible Encapsulant Emerson & Cuming 4640-25 Stycast® Two-Component Silicone Flexible EncapsulantDescriptionAn RTV condensation cure. Pourable and room temperature curable.FeaturesHigh TemperaturePoor Chemical Resista.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | ASTM D149 |
Devcon Zip Patch™ Epoxy Emergency Repair ProductsComments: High-technology, adhesive-impregnated, putty patching system that cures at room temperature. Hardens to a tough, durable, waterproof finish in minutes. Easy-to-u.. |
|||
Dielectric Strength | 9.84 kV/mm | 250 kV/in | |
Permabond 262 Cyanoacrylate PERMABOND 262 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 262 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates.. |
|||
Dielectric Strength | >= 9.84 kV/mm | >= 250 kV/in | |
Aremco Ceramacast™ 905 Silicon-Ceramic Potting Compound Ceramacast™ 905 is a silicone-bonded, ceramic filled high temperature adhesive and potting compound. |