Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Cyanoacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Overview of materials for Cyanoacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.875 - 2.24 g/cc
0.0316 - 0.0809 lb/in³
Average value: 1.11 g/cc Grade Count:307
Volatile Organic Compounds (VOC) Content 144 - 840 g/l
144 - 840 g/l
Average value: 527 g/l Grade Count:32
Particle Size 1.65 - 2.80 µm
1.65 - 2.80 µm
Average value: 2.13 µm Grade Count:3
pH 6.80 - 8.90
6.80 - 8.90
Average value: 8.09 Grade Count:4
Viscosity 0.400 - 1.10e+6 cP
0.400 - 1.10e+6 cP
Average value: 17700 cP Grade Count:373
Thickness 12.7 - 140 microns
0.500 - 5.50 mil
Average value: 63.0 microns Grade Count:24
Mechanical Properties Metric English Comments
Hardness, Barcol 65.0
65.0
Average value: 65.0 Grade Count:13
Hardness, Shore A 72.0 - 85.0
72.0 - 85.0
Average value: 84.0 Grade Count:13
Hardness, Shore D 27.0 - 85.0
27.0 - 85.0
Average value: 72.6 Grade Count:69
Tensile Strength, Ultimate 2.48 - 42.1 MPa
360 - 6100 psi
Average value: 25.2 MPa Grade Count:66
Tensile Strength, Yield 12.4 - 19.3 MPa
1800 - 2800 psi
Average value: 18.0 MPa Grade Count:71
Elongation at Break 2.00 - 340 %
2.00 - 340 %
Average value: 126 % Grade Count:47
Modulus of Elasticity 0.0111 - 2.76 GPa
1.61 - 400 ksi
Average value: 1.23 GPa Grade Count:13
Shear Strength 3.00 - 28.8 MPa
435 - 4180 psi
Average value: 20.3 MPa Grade Count:37
Adhesive Bond Strength 0.690 - 35.0 MPa
100 - 5080 psi
Average value: 15.7 MPa Grade Count:238
Peel Strength 0.0219 - 12.0 kN/m
0.125 - 68.5 pli
Average value: 2.82 kN/m Grade Count:38
Thermal Properties Metric English Comments
CTE, linear 55.0 - 162 µm/m-°C
30.6 - 90.0 µin/in-°F
Average value: 87.4 µm/m-°C Grade Count:106
Thermal Conductivity 0.100 - 1.65 W/m-K
0.694 - 11.5 BTU-in/hr-ft²-°F
Average value: 0.205 W/m-K Grade Count:97
Melting Point 160 - 170 °C
320 - 338 °F
Average value: 165 °C Grade Count:3
Boiling Point 93.0 - 169 °C
199 - 336 °F
Average value: 131 °C Grade Count:4
Maximum Service Temperature, Air 21.1 - 371 °C
70.0 - 700 °F
Average value: 120 °C Grade Count:340
Softening Point 149 - 155 °C
300 - 311 °F
Average value: 149 °C Grade Count:14
Minimum Service Temperature, Air -184 - -20.0 °C
-300 - -4.00 °F
Average value: -54.5 °C Grade Count:304
Glass Transition Temp, Tg -33.0 - 120 °C
-27.4 - 248 °F
Average value: 44.7 °C Grade Count:18
Flash Point -1.11 - 110 °C
30.0 - 230 °F
Average value: 64.1 °C Grade Count:36
Optical Properties Metric English Comments
Refractive Index 1.38 - 1.49
1.38 - 1.49
Average value: 1.47 Grade Count:17
Transmission, Visible 80.0 - 90.0 %
80.0 - 90.0 %
Average value: 80.2 % Grade Count:50
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+13 - 1.50e+16 ohm-cm
2.00e+13 - 1.50e+16 ohm-cm
Average value: 3.68e+15 ohm-cm Grade Count:18
2.50e+12 - 2.50e+12 ohm-cm

@Temperature 65.0 - 65.0 °C
2.50e+12 - 2.50e+12 ohm-cm

@Temperature 149 - 149 °F
Average value: 2.50e+12 ohm-cm Grade Count:3
Surface Resistance 0.0250 - 1.88e+17 ohm
0.0250 - 1.88e+17 ohm
Average value: 2.14e+16 ohm Grade Count:12
Insulation Resistance 2.50e+14 - 8.00e+14 ohm
2.50e+14 - 8.00e+14 ohm
Average value: 5.90e+14 ohm Grade Count:5
Shielding Effectiveness 57.0 - 85.0 dB
57.0 - 85.0 dB
Average value: 70.9 dB Grade Count:3
Dielectric Constant 2.50 - 4.60
2.50 - 4.60
Average value: 3.41 Grade Count:76
Dielectric Strength 9.84 - 303 kV/mm
250 - 7700 kV/in
Average value: 25.4 kV/mm Grade Count:105
Dielectric Breakdown 1500 - 8400 V
1500 - 8400 V
Average value: 2990 V Grade Count:7
Dissipation Factor 0.0100 - 0.0200
0.0100 - 0.0200
Average value: 0.0112 Grade Count:8
Processing Properties Metric English Comments
Processing Temperature 20.0 °C
68.0 °F
Average value: 20.0 °C Grade Count:30
Cure Time 0.0167 - 43200 min
0.000278 - 720 hour
Average value: 492 min Grade Count:280
3.00 - 60.0 min

@Temperature 60.0 - 170 °C
0.0500 - 1.00 hour

@Temperature 140 - 338 °F
Average value: 25.8 min Grade Count:12
Users viewing this material also viewed the following: