Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Compression Grade

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Sumitomo Bakelite High Peformance Plastics
Trade Name Sumikon®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Compression Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimensional stability with excellent heat resistance. Typical applications include brush holders for high temperature, and timing pulleys.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.02 g/cc
2.02 g/cc
ASTM D792
Bulk Density 0.960 g/cc
0.0347 lb/in³
ASTM D1895
Water Absorption 0.030 %
0.030 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D6289
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ASTM D638
Tensile Modulus 25.5 GPa
3700 ksi
ASTM D638
Flexural Strength 131 MPa
19000 psi
ASTM D790
Compressive Strength 241 MPa
35000 psi
ASTM D695
Izod Impact, Notched 0.214 J/cm
0.401 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Dielectric Constant 4.9

@Frequency 1e+6 Hz
4.9

@Frequency 1e+6 Hz
ASTM D150
5.0

@Frequency 1000 Hz
5.0

@Frequency 1000 Hz
ASTM D150
5.1

@Frequency 60 Hz
5.1

@Frequency 60 Hz
ASTM D150
Dielectric Strength 9.84 kV/mm
250 kV/in
Step by Step; ASTM D149
15.0 kV/mm
380 kV/in
Short Time; ASTM D149
Dissipation Factor 0.030

@Frequency 1000 Hz
0.030

@Frequency 1000 Hz
ASTM D150
0.030

@Frequency 1e+6 Hz
0.030

@Frequency 1e+6 Hz
ASTM D150
0.040

@Frequency 60 Hz
0.040

@Frequency 60 Hz
ASTM D150