Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | Z Direction, 50% RH; IPC-TM-650 2.5.6.2 |
Rogers Corporation RO4450B Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | Z Direction, 50% RH; IPC-TM-650 2.5.6.2 |
Rogers Corporation RO4450F Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC-TM-650.2.5.6.2 |
Park Electrochemical Nelco® N4000-7 EF® Halogen-Free Epoxy The Nelco® N4000-7 EF® series of laminates and prepregs is a total environmental solution. This advanced halogen-free resin system provides superior CAF resistance for high temperature, lead-free .. |
|||
Dielectric Strength | 39.4 - 78.7 kV/mm @Thickness 0.0762 mm |
1000 - 2000 kV/in @Thickness 0.00300 in |
|
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Dielectric Strength | >= 39.4 kV/mm | >= 1000 kV/in | DC |
Gwent Electronic Materials D2121102P1 UV Curable Dielectric Ink Screen printable UV cured green dielectric ink with good printability and excellent flexibility. Provides excellent screen life and is suitable for use with automated reel to reel, semi-automatic or.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D419 |
Teknor Apex Telcar® TL-1522H Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Dielectric Strength | >= 39.4 kV/mm | >= 1000 kV/in | At 20 mils; ASTM D149 |
Borealis Borstar® ME6052 Black Bimodal MD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar ME6052 is a black, bimodal, medium-density polyethylene compound produced using the Borstar process. It is characterized by its tailor-made properties important in jacketing applications, i.. |
|||
Dielectric Strength | >= 39.4 kV/mm | >= 1000 kV/in | At 20 mils; ASTM D149 |
Borealis Borstar® ME6053 Black Bimodal MD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar ME6053 is a natural, bimodal medium-density polyethylene compound produced using the Borstar process. It is characterized by its tailor made properties important in jacketing applications, .. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | Standard Condition; ASTM D1000 |
3M 1400 Economy Vinyl Electrical Tape 3M™ Economy Vinyl Electrical Tape 1400 is a black 7 mil thick, general use vinyl-insulating tape. It is designed to perform continuously in temperatures up to 80°C. This tape has a polyvinyl chlor.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg 85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Dielectric Strength | >= 39.4 kV/mm | >= 1000 kV/in | ASTM D149 |
Arlon CuClad 6250 Bonding Film Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System MULTICLAD™ HF represents the next generation low-loss thermoset and prepreg system for high-speed and high-frequency printed circuit boards. This technology combines a low-loss, high reliability t.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D149 |
Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D149 |
Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 8 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Prim.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 12 to 14 mil coating; ASTM D149 |
3M Scotchcast™ 260 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 12 to 15 mil coating; ASTM D149 |
3M Scotchcast™ 263 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 263 is a widely used, well-known general purpose epoxy powder resin. A one part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | |
Astro Met Macor® Machinable Glass Ceramic General Description:Macor is a machinable glass-ceramic material with a unique combination of useful properties. A product of Corning Incorporated, it is stocked, distributed and fabricated by Astro.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | Arlon SQA-TMS-020 |
Arlon 51581B015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon 51N Lead-Free Compatible Epoxy Low-Flow 51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stabili.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal .. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 35% RH |
3M Novec™ 1700 Electronic Grade Coating 3M™ Novec™ 1700 Electronic Grade Coating is designed for the protection of printed circuit boards and electronic components. It is a clear, low viscosity solution of a 2 wt% fluorochemical acrylic.. |
|||
Dielectric Strength | 39.4 kV/mm @Thickness 2.54 mm |
1000 kV/in @Thickness 0.100 in |
|
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | DC |
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C) |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 12 to 14 mil coating; ASTM D149 |
3M Scotchcast™ 260 CG Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D149 |
Arlon 44981R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene UL Recognition File: E54153.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D149 |
Arlon T1012-R004-xx 0.012" Self-Fusing Silicone Rubber Tape 1 inch wide, 12 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D149 |
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc.. |