Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.6 kV/mm | 600 kV/in | in oil; ASTM D149 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | |
Dow Questra® EA513 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | |
Dow Questra® WA551 High Heat Syndiotactic Polystyrene, 40% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | |
Dow Questra® WA552 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Short Term; ASTM D149 |
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Perpendicular, short time in oil; ASTM D149 |
Haysite H515 Polyester, High Temp Flex H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high t.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Perpendicular in Oil; ASTM D149 |
Haysite HTF Polyester, High Temp Flex HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 3.20 mm |
599 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 and 5VA listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInfo.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF33 TL15 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInfo.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 3.17 mm |
600 kV/in @Thickness 0.125 in |
|
Master Bond MasterSil 708FR One Part, Flame Resistant Silicone Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of .. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Westlake Plastics Propylux® Polypropylene Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance it abrasion. These properties makes it suitable f.. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PAI Polyamide-imide Particularly used where high strength in a wide range of temperature (-190°C…+260°C), high notched strength and very good dielectric properties are required. Features good chemical stability, fl.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Arlon 51106RB015D Silicone Rubber/Fiberglass Laminate Interleave 2: 3 mil PE; Side 2: cured silicone rubber; Substrate: 7628 fiberglass; Side 1: uncured silicone rubber, Interleave 1: 3 mil PE |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Arlon 51228R025 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Arlon 51756R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | |
3M Temflex™ 2155 Rubber Splicing Tape Temflex 2155 Rubber Splicing Tape is a conformable self-fusing rubber electrical insulating tape. It is designed for low voltage electrical insulating and moisture sealing applications. Temflex 2155.. |
|||
Dielectric Strength | >= 23.6 kV/mm | >= 600 kV/in | ASTM D149a |
Technetics Group Texolon™ 8764 PTFE
(Unverified Data**) A premium PTFE sheet manufactured from the highest quality PTFE.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectri.. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | ASTM D149 |
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | Average value: 23.6 kV/mm Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: SyndiotacticAppearance: BlackInformation provided by TP Composites, Inc. |