Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Questra® EA513 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Syndiotactic Polystyrene (SPS) , Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Questra® EA513 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are very different from conventional styrenics in structure, and properties, exhibiting excellent heat resistance with a melting temperature of 270.C, excellent moisture and chemical resistance together with a unique combination of exceptional electrical properties, toughness and processability. QUESTRA crystalline polymers are typically used as moldings, films, and fibers in Electronic, Electrical, Automotive, Consumer and Industrial, Filtration, Optical/photographic film and Specialty fiber/non-woven markets.QUESTRA EA513 is a 30% glass filled, ignition resistant polymer suitable for Electrical and Electronic applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM Data
Water Absorption 0.010 %
0.010 %
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 95.1 MPa
13800 psi
ASTM Data
Tensile Strength, Yield 95.1 MPa
13800 psi
ASTM Data
Tensile Modulus 9.65 GPa
1400 ksi
ASTM Data
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM Data
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.5 µm/m-°C

@Temperature 20.0 °C
16.9 µin/in-°F

@Temperature 68.0 °F
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 263 °C
505 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
Unannealed; ASTM Data
Vicat Softening Point 263 °C
505 °F
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Dielectric Strength 23.6 kV/mm
599 kV/in
Dissipation Factor 0.0010
0.0010