Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.0 kV/mm | 584 kV/in | |
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Network Polymers Kepital® F20-25 Description: Natural Acetal Copolymer, 25% Glass Reinforced GradeInformation provided by Network Polymers Inc. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 3.20 mm |
584 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.50 mm |
584 kV/in @Thickness 0.0984 in |
IEC 60243-1 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.00 mm |
584 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.00 mm |
584 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.00 mm |
584 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical Lupox® GP2300R PBT+GF30% Description: Injection Molding, PBT+GF30%, Anti-HydrolysisApplication: E&E (Speed Nut & Body)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI) Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
ASTM D149 |
Toyobo T-400 Nylon, 15% Glass-Reinforced Key Feature: G.F. 15%Information provided by Toyobo Co., Ltd |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243-1 |
DSM Arnitel® EM740 74 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | dry; IEC 60243-1 |
DSM Novamid® 1010GN2-30 NAT/BK37 PA6-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | dry; IEC 60243-1 |
DSM Novamid® 1015GH35 BK37 PA6-GF35 35% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | dry; IEC 60243-1 |
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.59 mm |
584 kV/in @Thickness 0.0625 in |
|
Cytec EN-2534 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243 |
Azoty Tarnow™ TARNOFORM 300 TF4 POM Tribological modified grade with addition of 20% PTFE, with very low coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.00 mm |
584 kV/in @Thickness 0.0394 in |
ASTM D149 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
ASTM D149 |
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
ASTM D149 |
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Dielectric Strength | 23.0 - 25.0 kV/mm | 584 - 635 kV/in | DIN 53481 |
Isoflon PAI Polyamideimide Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243-1 |
Lanxess Pocan® S 7020 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |