Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.8 kV/mm | 350 kV/in | Short Term; ASTM D149 |
Quadrant EPP Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet) |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Resinlab® CYNERGY CA6404 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Resinlab® CYNERGY CA6405 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | ASTM D149 |
Plenco 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 7000 is the replacement material for the former Union Carbide BMM-7000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding and preheating characteristics.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure, Black Information provided by ITW Devcon |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
ITW Devcon Rubber Repair / Castable Urethane High Temp Edge & Seal (T-36), Amber Information provided by ITW Devcon |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | Short Term |
Saint-Gobain Rulon® II Bearing/Seal PTFE An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | Wet, step-by-step. ASTM D149 |
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf.. |
|||
Dielectric Strength | 13.8 kV/mm @Frequency 60.0 Hz |
351 kV/in @Frequency 60.0 Hz |
Wet, step by step; ASTM D149 |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | step-by-step; ASTM D149 |
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Cytec (Conap) FR-1050 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Dow Corning 3-4222 DIELECTRIC FIRM GEL KIT Two-part, translucent green, firm, fast RT or heat cure, and primerless chemical adhesion.Information provided by Dow Corning |
|||
Dielectric Strength | 13.8 - 17.7 kV/mm @Thickness 3.17 mm |
350 - 450 kV/in @Thickness 0.125 in |
Short time value |
Abatron AboCast/AboCure 8109-6 High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 55989R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Arlon R30370A008 0.008" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Dielectric Strength | 13.8 - 14.6 kV/mm | 350 - 370 kV/in | Step by Step |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Dielectric Strength | 13.8 - 14.6 kV/mm | 350 - 370 kV/in | Short Time |
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | Short Time |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | Short Time |
Bulk Molding Compounds BMC 5307 Mineral Filled, Glass Reinforced Polyester BMC 5307 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a medium impact material produced in .. |
|||
Dielectric Strength | 13.8 - 15.7 kV/mm | 350 - 400 kV/in | Short Time |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass Data provided by the manufacturer, Owens Corning. |