Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
Manufacturer | Quadrant Engineering Plastics Products |
Trade Name | Nylatron® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Quadrant EPP Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
Water Absorption | 0.30 % | 0.30 % | Immersion, 24hr; ASTM D570(2) |
Water Absorption at Saturation | 5.5 % | 5.5 % | Immersion; ASTM D570(2) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 75 | 75 | ASTM D785 |
Tensile Strength | 93.1 MPa | 13500 psi | ASTM D638 |
Elongation at Break | 5.0 % | 5.0 % | ASTM D638 |
Tensile Modulus | 4.65 GPa | 675 ksi | ASTM D638 |
Flexural Strength | 145 MPa | 21000 psi | ASTM D790 |
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Compressive Strength | 124 MPa | 18000 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 4.14 GPa | 600 ksi | ASTM D695 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 36.0 µm/m-°C @Temperature -40.0 - 149 °C |
20.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM F433 |
Melting Point | 260 °C | 500 °F | Crystalline, Peak; ASTM D3418 |
Maximum Service Temperature, Air | 104 °C | 220 °F | Long Term |
Deflection Temperature at 1.8 MPa (264 psi) | 204 °C | 400 °F | ASTM D648 |
Flammability, UL94 | V-2 | V-2 | 1/8 inch (Estimated Rating) |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+13 ohm | 1.00e+13 ohm | EOS/ESD S11.11 |
Dielectric Strength | 13.8 kV/mm | 350 kV/in | Short Term; ASTM D149 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | No | No | |
Canada AG | No | No | |
FDA | No | No | |
NSF | No | No | |
USDA | No | No | |
USP Class VI | No | No |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Unacceptable | Unacceptable | |
Acids, Weak | Limited | Limited | |
Alcohols | Limited | Limited | |
Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
Alkalies, Weak | Limited | Limited | |
Chlorinated Solvents | Limited | Limited | |
Conductive / Static Dissipative | No | No | |
Continuous Sunlight | Limited | Limited | |
Hot Water / Steam | Limited | Limited | |
Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
Hydrocarbons - Aromatic | Acceptable | Acceptable | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Acceptable | Acceptable |
Descriptive Properties | Value | Comments |
---|---|---|
Machinability | 4 | 1-10, 1=Easier to Machine |