Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resinlab® CYNERGY CA6404 Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Resinlab®
Trade Name CYNERGY
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Resinlab® CYNERGY CA6404 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impart superior hot strength, impact and thermal resistance making them ideal for demanding applications.Application: The CYNERGY SERIES of the cyanoacrylates should be applied in small amounts to one surface only. The parts should then be mated together under slight pressure. This causes the adhesive to spread out into a thin film and assures optimum adhesive performance. The pressure need only be applied for several seconds. The CYNERGY SERIES cures rapidly allowing for bonded parts to be handled within 10 to 60 seconds for most applications. Full cure is normally within 24 hours.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Viscosity 4000 cP
4000 cP
Mechanical Properties Metric English Comments
Shear Strength 25.9 MPa
3750 psi
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C
36.1 µin/in-°F
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 3.5
3.5
Dielectric Strength 13.8 kV/mm
350 kV/in
Processing Properties Metric English Comments
Cure Time >= 0.300 min
>= 0.00500 hour
Fixture
480 min
8.00 hour
Full cure
Descriptive Properties Value Comments
Base Ethyl
Color Clear
Gap Fill (mil) 10