Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | PLC code 2; UL 746A |
SABIC Innovative Plastics Cycoloy® C1950 PC+ABS Low viscosity injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 103 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 121 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 123 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 201 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 201R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 223 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific) 10.5 MFR. Improved flame retardance. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746 |
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® FXM121R PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® LS3 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Medium-high viscosity. UV-stabilized. Adhesion to coatings. Transparent colors only. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 80.0 mm/min | 0.394 - 3.15 in/min | Average value: 37.1 mm/min Grade Count:13 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 143 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 144 PC (Asia Pacific) LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 1000R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | PLC code 2; UL 746A |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 1010F PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | PLC code 2; UL 746A |
SABIC Innovative Plastics Ultem 1010RV PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | PLC code 2; UL 746A |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2110 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2200 PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2200R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | PLC code 2; UL 746A |
SABIC Innovative Plastics Ultem 2313 PEI 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region... |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Valox® 830 PBT (Asia Pacific) 30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC (Asia Pacific) Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |