10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Melt Flow 11.3 g/10 min

@Load 6.60 kg,
Temperature 337 °C
11.3 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 114 MPa
16500 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 6.0 %
6.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 4.61 GPa
669 ksi
5 mm/min; ASTM D638
Flexural Strength 199 MPa
28900 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 5.24 GPa
760 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
4.00 J/cm

@Thickness 3.20 mm
7.49 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 207 °C

@Thickness 6.40 mm
405 °F

@Thickness 0.252 in
unannealed; ASTM D648
Glass Transition Temp, Tg 217 °C
423 °F
UL RTI, Electrical 170 °C
338 °F
UL 746B
UL RTI, Mechanical with Impact 170 °C
338 °F
UL 746B
UL RTI, Mechanical without Impact 170 °C
338 °F
UL 746B
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
UL 94
5VA

@Thickness 1.90 mm
5VA

@Thickness 0.0748 in
UL 94
Electrical Properties Metric English Comments
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten; ASTM D495
Comparative Tracking Index 100 - 175 V
100 - 175 V
UL 746A
Hot Wire Ignition, HWI 60 - 120 sec
60 - 120 sec
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
0.00 - 15 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min
1.00 - 3.15 in/min
UL 746A