Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 25.9 sec Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 24.1 sec Grade Count:15 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC 1 |
PTS Tristar® PC-30GFR 30% Glass Reinforced Polycarbonate Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Hot Wire Ignition, HWI | 15.0 - 120 sec | 15.0 - 120 sec | Average value: 72.9 sec Grade Count:22 |
Overview of materials for PVC, Flexible Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 1.50 mm |
60 - 120 sec @Thickness 0.0591 in |
UL 746A |
Idemitsu Kosan Xarec® EA 522 SPS, 22% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1010R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1100V PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2100F PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized col.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2212EPR PEI 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2300R PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2310R PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2312 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem MD131A PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 508 PBT+PC 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 508R PBT+PC 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-FR. Reduced warpage characteristics. Applications same as VALOX 420R. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 780 PBT 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4103 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4107 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL Rating PLC 1 (60-120 sec) |
Covestro Bayblend® FR 90 N Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sepa.. |
|||
Hot Wire Ignition, HWI | 15.0 - 120 sec | 15.0 - 120 sec | Average value: 75.3 sec Grade Count:26 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.05 mm |
60 - 120 sec @Thickness 0.120 in |
UL PLC 1 |
Resinoid 1322 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |